Seat Heating PET Film Elements for 80-120 °C

Which insulation systems hold 80 °C to 120 °C continuously, what this construction is rated to, and the control and cut-out that hold the surface there.

Seat Heating PET Film Elements are rated 120 °C continuous, a limit set by the PET polyester film, which covers 80 °C to 120 °C. Battery operating windows, incubators, fluid warming and display heating. The upper limit of PET film, and the band where a low-cost printed heater stops being a candidate.

Working band
80 °C to 120 °C
Continuous limit, this construction
120 °C
Set by
PET polyester film
Watt density
0.05 W/cm² free air, 0.25 W/cm² bonded
Total thickness
0.3 mm with facing
Maximum outline, one piece
500 x 600 mm per element

The band is the temperature the heated surface has to hold, not the temperature the element reaches. The element always runs hotter, by an amount the watt density and the thermal path decide, so the cut-out is set against the element and not against the load.

Seat Heating PET Film Elements — the construction this guide is about

Working temperature page for seat heating pet film elements at 80 °c to 120 °c. What survives this band, what stops just below it, why the boundary is where it is, and how the temperature is actually measured and held.

What the 80 °C to 120 °C Band Requires

Battery operating windows, incubators, fluid warming and display heating. The upper limit of PET film, and the band where a low-cost printed heater stops being a candidate.

Band80 °C to 120 °C
This construction, continuous120 °C
Limited byPET polyester film

This band reaches the ceiling of the construction. At 120 °C there is no headroom left, so the control has to hold the set point rather than approach it from above, and the limit device has to be set where it can act before the insulation does. A duty that spends its time at the top of the band is a duty that should be quoted against the next construction up.

Why the Boundary Is Where It Is

120 °C is where PET film stops. The polyester softens from about 130 °C and loses its dielectric strength as it softens, so the margin between working temperature and failure is thin — and a failure here is an electrical one, not a cosmetic one.

This is therefore the last band in which the cheapest thin heater is a candidate. Above it, the construction changes to silicone or polyimide, and the cost per square metre changes with it.

What a Seat Heating PET Film Elements Is

Carbon film elements shaped to a seat cushion and backrest, perforated for breathability and terminated for an automotive harness.

Carbon or silver ink screen printed onto PET polyester film, laminated and die cut. It is made on a roll, which makes it the cheapest heater per square metre by a wide margin at volume, and it stops at 120 °C because the film does. Automotive elements are built at very low watt density over a large area — a seat pad or a mirror face — where comfort, not process temperature, is the duty.

The heat leaves through the bonded face. Everything that is not in contact with the load radiates and convects from the back of the heater instead, which at these thicknesses is a poor path — so an air gap under part of the outline is not a small loss of efficiency, it is a hot spot at that spot.

Elementscreen-printed carbon or silver ink
Insulation systemPET polyester film
Total thickness0.3 mm with facing
Maximum size, one piece500 x 600 mm per element
Continuous working temperature120 °C

The continuous limit of 120 °C is set by PET polyester film. The element alloy would run far hotter; it is never the element that decides.

Which Temperature Is Being Held

Three temperatures matter and they are not the same number: the element temperature, the temperature of the surface being heated, and the ambient. A heater rated for a continuous working temperature is rated at the element — the hottest point in the assembly, and the one nothing on the outside is measuring.

The gap between element and surface is the thermal path. Bonded to metal it may be a few degrees; across an air gap, a void in the adhesive or a dry clamped joint it can be tens of degrees, and every one of them appears at the element rather than at the load.

Which is why sensor position is a drawing item. A sensor laminated into the heater protects the heater; a sensor on the load controls the load. Assemblies that have to do both carry two: a control sensor where the process is, and a limit device against the element.

Watt Density: the Two Figures

This construction is rated at 0.05 W/cm² in free air and 0.25 W/cm² bonded over its whole area to metal. The second figure is 5 times the first, and the difference is not a safety margin — it is the heat sink. On a 100 x 150 mm outline, which is 150 cm², that is about 8 W hanging in air against about 38 W bonded down.

Specify at the figure that matches how the heater will actually run. A heater ordered at the bonded density and then switched on before it is attached — on the bench, during a test, after it has lifted off in service — reaches its insulation limit in minutes, because there is nowhere for the heat to go but through the insulation.

Control and Protection

This heater has no way of limiting its own temperature. Resistance heating draws roughly the same power whatever the temperature, so with the load removed, the fluid gone, the fan stopped or the sensor open circuit, the element keeps producing watts until something stops it.

The design must therefore contain a control device and, separately, a protective one: a controller with a sensor to hold the set point, and a bimetal thermostat or a one-shot thermal cutoff wired in series with the element to open the circuit if the loop ever fails. The two are not interchangeable — a controller that has lost its sensor cannot protect anything, which is exactly the fault the cutoff exists for.

PET softens at about 130 °C and loses its dielectric strength as it does, so the cutoff temperature has to sit under that with margin. This is a construction that cannot be allowed to dry out and overshoot.

Sensors can be built into the part: NTC thermistor, PT100 or PT1000 RTD, or a K-type thermocouple, fitted under the same insulation and tested with the heater as one assembly. A sensor laminated into the heater reads the heater; a sensor on the load reads the load. Both are legitimate, and the drawing has to say which is wanted.

How This Construction Fails

  • Run at the bonded watt density in free air. The insulation reaches its limit within minutes and the element burns through where the local density is highest. Specify at 0.25 W/cm² only where the heater is genuinely bonded to metal over its whole area; unbonded, the figure is 0.05 W/cm².
  • Voids under the bond. Air trapped during application, a contaminated surface or an adhesive that never reached full cure all produce the same result: a patch with no thermal path, running far above the rest of the heater, which is where the failure starts.
  • Loss of the control loop. An open-circuit sensor, a welded relay contact or a controller in manual leaves the element at full power with nothing watching it — the case the series thermal cutoff exists for, and the reason it must not be omitted to save a part.
  • Overshoot into the film. PET softens from about 130 °C and its dielectric strength goes with it, so a fault that a silicone heater shrugs off destroys a PET element.
  • Silver migration. A printed silver circuit under a DC bias, in humidity, grows dendrites between adjacent tracks; carbon does not, which is one reason carbon is still used where the geometry allows it.

Where This Construction Is the Wrong Answer

  • Do not plan on running above 120 °C. That ceiling belongs to the insulation system, not to the element alloy, and it is not a figure that derating extends — past it the insulation degrades and the dielectric strength goes with it.
  • Do not use PET film for process heat. At 120 °C it is at its ceiling, and the constructions that go above it — silicone, polyimide, thick film — are different parts, not the same part with a different rating.

How to Specify One

This is a made-to-drawing part, so there is no catalogue number to quote. A quotation is built from the following, and the more of it that arrives with the enquiry the fewer rounds it takes:

  • An outline drawing, or a sketch with dimensions: overall size, holes, cut-outs, radii and the lead exit position.
  • The supply voltage, and whether it is AC or DC. The element is wound for one voltage; it is not a switchable range.
  • The power required, or — better — the temperature to be reached and the mass or flow it has to be reached in. Given the second, the wattage can be calculated instead of guessed.
  • What the heater is attached to, and how. This is what decides which watt density figure applies, and it is the question a quotation cannot proceed without.
  • The ambient, and the lowest temperature the assembly must start from. A heater sized for a 20 °C start is undersized for a -30 °C one.
  • Duty cycle: continuous, intermittent, or a warm-up to a deadline. Time to temperature is a specification, not a by-product.
  • Sensor and protection: which sensor, where it goes, and which limit device is fitted in series with the element.
  • The certification the end product is built to, named on the enquiry rather than after approval.
  • Quantity and target price, because the construction that is right for fifty pieces is often not the one that is right for fifty thousand.
  • Whether adhesive backing is wanted, and what surface it goes onto — a low-energy plastic needs a different adhesive from bare aluminium.

Lead time: Samples 7-10 days from approved drawing; production 15-20 days.

Seat Heating PET Film Elements — Capability Table

These are process limits for the construction, not the specification of one stocked item. Every line is what the factory can hold; what your part holds is fixed on your drawing.

ParameterSpecificationLimit / note
ConstructionCarbon ink on PET, perforated, with a non-woven faceDecided at quotation from the outline and the wattage
Insulation systemPET polyester film, 0.05 mm to 0.125 mm per faceThis is what sets the temperature limit, not the element
Total thickness0.3 mm with facingNominal, before adhesive; add 0.2 mm for PSA backing
Minimum size20 x 20 mmBelow this the element cannot be routed with a safe edge margin
Maximum size, one piece500 x 600 mm per elementLarger areas are supplied as tiled zones with separate circuits
Dimensional toleranceu00b11 mm on the die-cut outlineOn the die-cut outline; hole positions are held tighter
Supply voltage12 V, 24 VWound to the ordered voltage u2014 it is not a switchable range
Resistance toleranceu00b110% standard, u00b15% on requestMeasured at 20 u00b0C; hot resistance differs with the element alloy
Watt density, free air0.05 W/cmu00b2 typicalNothing conducting heat away u2014 the honest figure for an unbonded heater
Watt density, bonded to heat sink0.25 W/cmu00b2 maximumOnly valid with full-area contact to metal; specifying at this figure and running in free air destroys the heater
Continuous working temperature-40 u00b0C to +120 u00b0C continuousOf the heater itself, measured at the element, not the ambient
Dielectric strength1500 V AC, 1 minuteOne minute, element to any exposed surface, no breakdown
Insulation resistancegreater than 100 Mu03a9At 500 V DC, measured after the dielectric test
Lead wireCrimped or soldered leads, or a printed silver bus bar with a bonded tailLength, gauge and termination to your drawing
AttachmentPSA backing standard; laminated into the end product at high volumeAdhesive-backed heaters need continuous contact pressure while curing
Sensor and control optionsNTC 10K B3950 bonded to the film, or a printed PTC ink trackFitted under the same insulation and tested as one assembly
Certifications availableIEC/EN 60335, UL 94 V-0, RoHS, REACH, CE, IATF 16949Constructions are built to these; the certificate covers the construction, not every outline
Comfort targetSurface at 35 u00b0C to 40 u00b0C within 3 minutesA seat heater is a comfort device u2014 the specification is the time to comfort, not the wattage
Bending fatigueSurvives 100,000 cushion compression cyclesWhich is what a printed element on PET is genuinely good at

Capability figures are for screen-printed carbon or silver ink on PET polyester film. The +120 °C continuous limit is the film's, and it is a hard limit: PET softens and loses dielectric strength above roughly 130 °C, so this construction is only a candidate where the maximum credible temperature is bounded well below it.

Outline & Specification Builder

Set the outline, the size, the voltage and the power you have in mind. The drawing redraws to match, and the panel works out the heated area, the watt density and the current — then checks that watt density against what this construction survives in free air and bonded to a heat sink. Those two limits are different by several times, and it is the difference that decides whether a heater lasts.

Fills in the form below; attach your outline drawing or DXF there.

Build the Drawing

The panel above checks whether a size and a wattage can be built. This is the drawing itself: set the outline, route the heating track, place the lead wires, terminals, connector and temperature sensor, working in PET / PTC film, and turn the model to look at it. When it is right, export the 2D drawing as a PDF or a DXF and send it with your enquiry — a drawing is what a quotation for seat heating pet film elements is actually written from.

HEATING FILM DRAWING
PET / PTC Film Heater

Draw the outline, route the heating track, place the lead exits, terminals and sensor, dimension it, then export a PDF or a DXF and send it with your enquiry. Nothing here is a stock part and nothing you draw commits you to anything.

CMD

Want to compare constructions before you draw? Open the full builder, where every film family is selectable in one place.

Our facility

Held in production, not just on paper

The limits above are the ones our own lamination press, die and test lines actually hold, and every unit is tested rather than a sample. A figure is only worth quoting if it survives the process that produces it.

Insulation film fed from the roll
Vulcanising press closing on a lay-up
Heater outlines being die cut
Finished heaters batched for dispatch

Request a Quote

The form below follows the current technical drawing configuration. Change the drawing values above and the request details update automatically.

Request a Quotation

The part

If you have an outline drawing or a DXF, say so in the notes and we will reply with an address to send it to — a drawing turns an estimate into a quotation.

Business Information

Dimensions & Specifications (IEC 60335 / UL 94 V-0 / RoHS)

ParameterSpecificationLimit / note
ConstructionCarbon ink on PET, perforated, with a non-woven faceDecided at quotation from the outline and the wattage
Insulation systemPET polyester film, 0.05 mm to 0.125 mm per faceThis is what sets the temperature limit, not the element
Total thickness0.3 mm with facingNominal, before adhesive; add 0.2 mm for PSA backing
Minimum size20 x 20 mmBelow this the element cannot be routed with a safe edge margin
Maximum size, one piece500 x 600 mm per elementLarger areas are supplied as tiled zones with separate circuits
Dimensional toleranceu00b11 mm on the die-cut outlineOn the die-cut outline; hole positions are held tighter
Supply voltage12 V, 24 VWound to the ordered voltage u2014 it is not a switchable range
Resistance toleranceu00b110% standard, u00b15% on requestMeasured at 20 u00b0C; hot resistance differs with the element alloy
Watt density, free air0.05 W/cmu00b2 typicalNothing conducting heat away u2014 the honest figure for an unbonded heater
Watt density, bonded to heat sink0.25 W/cmu00b2 maximumOnly valid with full-area contact to metal; specifying at this figure and running in free air destroys the heater
Continuous working temperature-40 u00b0C to +120 u00b0C continuousOf the heater itself, measured at the element, not the ambient
Dielectric strength1500 V AC, 1 minuteOne minute, element to any exposed surface, no breakdown
Insulation resistancegreater than 100 Mu03a9At 500 V DC, measured after the dielectric test
Lead wireCrimped or soldered leads, or a printed silver bus bar with a bonded tailLength, gauge and termination to your drawing
AttachmentPSA backing standard; laminated into the end product at high volumeAdhesive-backed heaters need continuous contact pressure while curing
Sensor and control optionsNTC 10K B3950 bonded to the film, or a printed PTC ink trackFitted under the same insulation and tested as one assembly
Certifications availableIEC/EN 60335, UL 94 V-0, RoHS, REACH, CE, IATF 16949Constructions are built to these; the certificate covers the construction, not every outline
Comfort targetSurface at 35 u00b0C to 40 u00b0C within 3 minutesA seat heater is a comfort device u2014 the specification is the time to comfort, not the wattage
Bending fatigueSurvives 100,000 cushion compression cyclesWhich is what a printed element on PET is genuinely good at

Video: Seat Heating PET Film Elements for 80-120 °C

Third-party video, selected automatically for this topic. It is not produced by Heating Film and is not a specification source — use the tables on this page for dimensional data.

Frequently Asked Questions

How large can one piece be?

500 x 600 mm per element in a single piece. Larger areas are supplied as tiled zones with separate circuits, which is usually better engineering anyway: separate zones can be controlled separately, and a large single circuit has to carry the whole current at one lead exit.

Which heaters work at 80 °c to 120 °c?

Battery operating windows, incubators, fluid warming and display heating. The upper limit of PET film, and the band where a low-cost printed heater stops being a candidate.

Is the temperature rating the surface temperature or the element temperature?

The element temperature, which is the hottest point in the assembly and the one nothing on the outside is measuring. The surface being heated sits below it by whatever the thermal path costs — a few degrees through a good bond, tens of degrees across a void or a dry clamped joint.

What watt density can seat heating pet film elements run at?

0.05 W/cm² with nothing conducting the heat away, and 0.25 W/cm² bonded over its whole area to metal. The two figures describe two different installations, not a range to choose from: a heater specified at 0.25 W/cm² and then run in free air reaches its insulation limit within minutes.

How do I request a quotation?

Send the outline drawing with the supply voltage, the power or the target temperature, what the heater is bonded to, the ambient and the duty cycle. We respond within one business day.